J. M. Pérez, R. Casasola, J.Ma. Rincón, M. Romero. Nucleation and crystallisation kinetics of a Na-fluorrichterite base glass by differential scanning calorimetry (DSC). Journal of Non-Crystalline Solids 358 (2012) 2741-2748.
J. M. Pérez, R. Casasola, J.Ma. Rincón, M. Romero. Nucleation and crystallisation kinetics of a Na-fluorrichterite base glass by differential scanning calorimetry (DSC). Journal of Non-Crystalline Solids 358 (2012) 2741-2748.